Effect of oxygen concentration on nanoindentation-induced phase transformations in ion-implanted amorphous silicon

  • S. Ruffell*
  • , J. Vedi
  • , J. E. Bradby
  • , J. S. Williams
  • , B. Haberl
  • *Corresponding author for this work

    Research output: Contribution to journalArticlepeer-review