Nanoindentation of metallic glasses

Tim Burgess*, M. Ferry

*Corresponding author for this work

    Research output: Contribution to journalReview articlepeer-review

    78 Citations (Scopus)

    Abstract

    Offering some of the highest specific strength and resilience values known among bulk materials, metallic glasses have the potential to revolutionize the field of materials science and engineering. Through effectively probing the fundamental mechanism responsible for deformation in these materials, nanoindentation has the potential to provide the answers necessary for their practical application.

    Original languageEnglish
    Pages (from-to)24-32
    Number of pages9
    JournalMaterials Today
    Volume12
    Issue number1-2
    DOIs
    Publication statusPublished - Jan 2009

    Fingerprint

    Dive into the research topics of 'Nanoindentation of metallic glasses'. Together they form a unique fingerprint.

    Cite this