Nanoindentation studies on waveguides inscribed in chalcogenide glasses using ultrafast laser

Tamilarasan Sabapathy, M. S.R.N. Kiran, Arunbabu Ayiriveetil, Ajoy K. Kar, U. Ramamurty, Sundarrajan Asokan*

*Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

10 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Nanoindentation studies on waveguides inscribed in chalcogenide glasses using ultrafast laser'. Together they form a unique fingerprint.
Sort by

Material Science

Physics