Post-deposition ageing reactions of plasma derived polyterpenol thin films

Kateryna Bazaka, Mohan V. Jacob*

*Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

39 Citations (Scopus)

Abstract

Owing to the structural flexibility, uncomplicated processing and manufacturing capabilities, plasma polymers are the subject of active academic as well as industrial research. Polymer thin films prepared from non-synthetic monomers combine desirable optical and physical properties with biocompatibility and environmental sustainability. However, the ultimate expediency and implementation of such materials will dependent on the stability of these properties under varied environmental conditions. Polyterpenol thin films were manufactured at different deposition powers. Under ambient conditions, the bulk of ageing occurred within first 150 h after deposition and was attributed to oxidation and volumetric relaxation. Films observed for further 12 months showed no significant changes in thickness or refractive index. Thermal degradation behaviour indicated thermal stability increased for the films manufactured at higher RF powers. Annealing the films to 405 °C resulted in full degradation, with retention between 0.29 and 0.99%, indicating films' potential as sacrificial material.

Original languageEnglish
Pages (from-to)1123-1128
Number of pages6
JournalPolymer Degradation and Stability
Volume95
Issue number6
DOIs
Publication statusPublished - Jun 2010
Externally publishedYes

Fingerprint

Dive into the research topics of 'Post-deposition ageing reactions of plasma derived polyterpenol thin films'. Together they form a unique fingerprint.